Physical Properties Metric English Comments
Specific Gravity 0.740 g/cc
0.740 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.4 MPa
2810 psi
ASTM D638
Flexural Modulus 0.8770 GPa
127.2 ksi
ASTM D790
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 71.1 °C
160 °F
ASTM D648