Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Diofan® A 063 Polyvinylidene Chloride (PVDC)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Diofan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® A 063 Polyvinylidene Chloride (PVDC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Coatings of Diofan® A 063 PVDC latex exhibit good adhesion on Corona treated polyolefin and PET films. The coatings are tack free. This grade is in particular recommended for the coating of extruded - laminated PE, and as an extrusion primer for PE on various substrates.Features: Moisture Barrier; Oxygen BarrierUses: Coating ApplicationsAdditional Properties: Density - 1.650 g/cm³; Density - 1.300 g/cm³; Emulsion Type - Anionic; Filmability - 19 °C; Heat Seal Maximum Resistance - 2.2 N/cm; Heat Seal Threshold - 107 °C; Oxygen Transmission Rate - ASTM D3985 21 cm³/m²/bar/24 hr; pH - 2.0; Shelf Life - (23°C): 10 month; Solids Content - 50 %; Surface Tension - 40 mN/m; Viscosity - (20°C): 8 mPa·sInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Water Vapor Transmission 37.0 g/m²/day

@Thickness 0.00100 mm,
Temperature 38.0 °C
2.38 g/100 in²/day

@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Mechanical Properties Metric English Comments
Coefficient of Friction, Dynamic 0.35
0.35
vs. Itself; ASTM D1894
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH); EU No 10/2011
Availability Asia Pacific
Europe
Latin America
North America
Color Milky White
Form Liquid