Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 37.0 g/m²/day @Thickness 0.00100 mm, Temperature 38.0 °C |
2.38 g/100 in²/day @Thickness 0.0000394 in, Temperature 100 °F |
90% RH; ASTM F1249 |
Solvay Specialty Polymers Diofan® A 063 Polyvinylidene Chloride (PVDC) Coatings of Diofan® A 063 PVDC latex exhibit good adhesion on Corona treated polyolefin and PET films. The coatings are tack free. This grade is in particular recommended for the coating of extru.. |