Solvay RHODOLINE® 697 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOLINE® 697 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© 697 is a defoamer especially formulated to give outstanding foam control when used in the manufacture of paints and coatings. In paint formulations, 2- 6 pounds of RHODOLINE© 697 will effectively defoam 100 gallons of paint, providing prolonged protection. RHODOLINE© 697 is not water-dispersible and should be used as received. For easy handling, RHODOLINE© 697 should be stored at temperatures above 50ºF, but not above 100ºF.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.840 - 0.980 g/cc
0.0303 - 0.0354 lb/in³
RP-17617
pH 7.0
7.0
0.05
Viscosity 800 - 1200 cP
800 - 1200 cP
#3 sp @ 60 rpm; RP-0596
Ash 2.0 - 2.5 %
2.0 - 2.5 %
RP-0065
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Opaque, White to Off-White Liquid
RP-0064
Hegman Test <6
Grind, RP-9186