Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.970 - 0.980 g/cc | 0.0350 - 0.0354 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet RGD525 High Temperature Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |
|||
Density | 0.914 - 0.980 g/cc | 0.0330 - 0.0354 lb/in³ | Average value: 0.945 g/cc Grade Count:71 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Density | 0.980 - 0.980 g/cc @Temperature 290 - 290 °C |
0.0354 - 0.0354 lb/in³ @Temperature 554 - 554 °F |
Average value: 0.980 g/cc Grade Count:1 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 0.970 - 0.980 g/cc | 0.0350 - 0.0354 lb/in³ | |
Solvay ALKAMULS® S 80 Surfactant Identification: SORBITAN MONOOLEATECAS: 1338 - 43 – 8EINECS: 215 – 665 – 4Available in: Asia Pacific, Europe, Latin America and North America. Solubility: Dispersible in water. Solub.. |
|||
Density | 0.840 - 0.980 g/cc | 0.0303 - 0.0354 lb/in³ | RP-17617 |
Solvay RHODOLINE® 697 Surfactant Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer.. |
|||
Density | 0.917 - 0.980 g/cc | 0.0331 - 0.0354 lb/in³ | ASTM D792 |
Plastic Lumber from the Plastic Lumber Co. Description: Plastic Lumber is a product similar to wood that is made from recycled plastic jugs. Products will never splinter, rot, crumble or need painting. Plastic Lumber has rapidly gained accep.. |
|||
Density | 0.968 - 0.979 g/cc | 0.0350 - 0.0354 lb/in³ | ASTM D4052 |
ExxonMobil Jayflex™ DINP Plasticizer (Asian Grade) Availability: Asia PacificCAS Number: 68515-48-0Information provided by ExxonMobil |
|||
Density | 0.910 - 0.980 g/cc | 0.0329 - 0.0354 lb/in³ | Average value: 0.921 g/cc Grade Count:189 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Density | 0.980 - 0.980 g/cc @Temperature 285 - 285 °C |
0.0354 - 0.0354 lb/in³ @Temperature 545 - 545 °F |
Average value: 0.980 g/cc Grade Count:1 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |