Solvay RHODAPEX® XEF/A Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPEX® XEF/A Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: AMMONIUM LAURETH/LAURYL SULFATE BLENDCAS: 67762-19-0, 2235-54-3Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX XEF/A is a versatile toiletry raw material which combines optimum performance with excellent foaming characteristics. The viscosity of these derived formulations can be adjusted by the addition of inorganic salts. The mildness of a product formulated with Rhodapex XEF/A may be improved by the inclusion of cocoampho-acetates, or high purity amphoterics like the MIRANOL ULTRA series. RHODAPEX XEF/A is used in many personal care applications such as hair shampoo, foam baths, shower products, liquid soaps, creams.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
pH 6.0 - 6.9
6.0 - 6.9
4% Solution; RP-17601
Optical Properties Metric English Comments
Transmission, Visible >= 95 %

@Wavelength 440 nm
>= 95 %

@Wavelength 440 nm
25% Active; RP-17605
Chemical Properties Metric English Comments
Ionic Impurities - Fe (Iron) <= 5.0 ppm
<= 5.0 ppm
RP-17610
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Hazy Liquid
RP-17620
Composition Active
69-71%, MW 347, RP-17102
Ammonium Chloride
<0.5%, RP-17504
Ammonium Sulfate
<0.75%, RP-17503
Citric Acid
0.3-0.8%, RP-17648
Unsulfate Matter
<2.5%, RP-17303
Odor Characteristic
Setting point 12°C