Material Notes:
Heavy metal free PVC compound recommended for extrusion of profiles for general purposes and flexible Sheet.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.19 - 1.25 g/cc
1.19 - 1.25 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 53 - 57

@Time 15.0 sec
53 - 57

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 11.1 MPa
>= 1610 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Descriptive Properties Value Comments
Application Flexible Sheet