Material Notes:
Description: Soluble in water and mineral oil. Exceptional stability in alkali. Outstanding compatibility in concentrated electrolyte solutions. Effective coupling agent for nonionic surfactants in liquid alkali detergent systems. Excellent textile wetting properties and hard surface detergency.Identification: POLYOXYETHYLENE ALKYL PHOSPHATE ESTER ACID FORMCAS: 68130 – 47 – 2Solubility: Soluble in water and in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Industrial cleaners (wetting and dispersing agent). Textile (emulsifier). Agrochemical formulations. Extreme-pressure additive for the formulation of soluble oils, semi-synthetic and synthetic fluids. Specially recommended for its anti-corrosion properties.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Thermal Properties Metric English Comments
Pour Point <= 0.000 °C
<= 32.0 °F
Flash Point >= 100 °C
>= 212 °F
Chemical Properties Metric English Comments
Total Acid Number 110 - 121
110 - 121
[mg KOH/g]; RPG44
Processing Properties Metric English Comments
Moisture Content <= 1.5 %
<= 1.5 %
RPG16
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear liquid
RPG31
Color <100 HU
Hazen, RPG23
Composition Active
0.99
Nonionic content
<9%, RPG35
Ionic Charge Anionic
Copyright © lookpolymers.com All Rights Reserved