Material Notes:
Aramid fibers with a SBR binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, steam, inert gases, mild acids and mild alkaliesInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0608 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 12.4 MPa
1800 psi
across grain; ASTM F152
Thermal Properties Metric English Comments
Thermal Conductivity 0.290 - 0.380 W/m-K
2.01 - 2.64 BTU-in/hr-ft²-°F
ASTM F433
Maximum Service Temperature, Air 371 °C
700 °F
204 °C

@Pressure 6.89 MPa
400 °F

@Pressure 1000 psi
Continuous
Minimum Service Temperature, Air -73.3 °C
-100 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 14.8 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 375 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
>= 26.7 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 678 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.03125 in. thickness; ASTM D149
Descriptive Properties Value Comments
Color Off-White
Compressibility, % 7-17
ASTM F36
Creep Relaxation, % 23
ASTM F38
Sealability ASTM F37B, ml/hr 1
ASTM Fuel A
2
Nitrogen