Material Notes:
Description: Soil Release Polymer offering protection against the adhesion of greasy soils between two wash cycles. 100% active material in powder form.Chemical Name: POLYETHYLENE GLYCOL POLYESTERCAS Number: 9016-88-0Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: REPEL-O-TEX© SRP-6 is a polymer offering protection against the adhesion of greasy soils to polyester fabrics after two wash cycles.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
Particle Size <= 300 µm
<= 300 µm
0.2
300 - 850 µm
300 - 850 µm
0.6
850 - 1180 µm
850 - 1180 µm
0.2
>= 1180 µm
>= 1180 µm
<1%
pH 4.0 - 8.0
4.0 - 8.0
1% Dispersion in Water; RP-0420
Viscosity <= 300 cP

@Temperature 176 °C
<= 300 cP

@Temperature 349 °F
Processing Properties Metric English Comments
Moisture Content <= 3.0 %

@Temperature 105 °C,
Time 3600 sec
<= 3.0 %

@Temperature 221 °F,
Time 1.00 hour
RP-0540
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clean Granules
RP-0064
Composition Polymer
>97%
Saponification number 98-109 mg KOH/g
RP-0496