Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 1180 µm | >= 1180 µm | <1% |
Solvay REPEL-O-TEX® SRP-6 Polyethylene Glycol Polyester Description: Soil Release Polymer offering protection against the adhesion of greasy soils between two wash cycles. 100% active material in powder form.Chemical Name: POLYETHYLENE GLYCOL POLYESTERCA.. |
|||
Particle Size | <= 1180 µm | <= 1180 µm | >95%; TI-2087 |
Solvay RHODOPOL® G Surfactant Description: Rhodopol® G is granular and dust free grade of Xanthan Gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent. It has rapid hydration propertie.. |
|||
Particle Size | <= 1180 µm | <= 1180 µm | >95%; TI-2087 |
Solvay RHODOPOL® TG Surfactant Description: Transparent, granular grade xanthan gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent.Identification: XANTHAN GUMCAS: 11138 – 66 – .. |