Solvay REPEL-O-TEX® PF-594 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay REPEL-O-TEX® PF-594 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High active soil release polymer for powder laundry. Prevents adhesion of soils between washes and soil redeposition during wash. Repel-O-Tex PF 594 has been specifically formulated for improved flowability and lower dust, providing ease of handling. The high, 96%, active level also improves cost-in-use versus 90% active Repel-O-Tex SF.Chemical Name: POLYAROMATIC ESTERAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: REPEL-O-TEX© PF-594 is a polymer offering protection against the adhesion of greasy soils between two wash cycles. 63% active material in powder form. Designed for anionic detergents.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.620 - 0.800 g/cc
0.0224 - 0.0289 lb/in³
RP-0155
Particle Size <= 25 µm
<= 25 µm
on #35 Mesh; RP-0499
<= 40 µm
<= 40 µm
Thru #100 Mesh; RP-0499
pH 3.0 - 6.0
3.0 - 6.0
1% Dispersion in Water; RP-0420
Processing Properties Metric English Comments
Moisture Content <= 2.0 %

@Temperature 105 °C,
Time 3600 sec
<= 2.0 %

@Temperature 221 °F,
Time 1.00 hour
RP-0540
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Off white free flowing powder
RP-0064
Composition Anticaking Agent
12/18/2012
Polymer
60-66%, RP-0065
Sodium Sulfate
19-25%, RP-0557