Solvay Chemicals Blanc fixe brilliant

Category Ceramic
Manufacturer Solvay Chemicals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Blanc fixe brilliant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blanc Fixe Brilliant is the optimal extender for almost all applications in the production of paints and coatings and plastic.Information provided by Solvay
Physical Properties Metric English Comments
Particle Size 0.80 µm
0.80 µm
Descriptive Properties Value Comments
Conductivity 80 µS/cm
Oil Index 13 g/100g