SolVin 263RB Polyvinyl Chloride General Purpose - Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer SolVin
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SolVin 263RB Polyvinyl Chloride General Purpose - Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Made by suspension polymerization. APPLICATIONS Blow extrusion : opaque or crystal-clear bottles Calendering : opaque or crystal-clear rigid sheets Extrusion : rigid profiles and filmsInformation provided by SolVin.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 0.30 g/l
<= 0.30 g/l
ISO 1269
Apparent Bulk Density 0.565 g/cc
0.0204 lb/in³
ISO 60
Particle Size 63 µm
63 µm
>95% greater than value; ISO 1624
250 µm
250 µm
<5% greater than value; ISO 1624
Viscosity Test 98 cm³/g
98 cm³/g
Reduced viscosity, K value = 63; ISO 1628-2