Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 98 cm³/g | 98 cm³/g | Reduced viscosity, K value = 63; ISO 1628-2 |
SolVin 263RB Polyvinyl Chloride General Purpose - Rigid Made by suspension polymerization.
APPLICATIONS
Blow extrusion : opaque or crystal-clear bottles
Calendering : opaque or crystal-clear rigid sheets
Extrusion : rigid profiles and filmsInformation pr.. |
|||
Viscosity Test | 98 cm³/g | 98 cm³/g | Viscosity number |
BASF Ultradur B 4406 G6 Q717 30% Glass Filled PBT Ultradur B 4406 G6 Q717 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |