Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 250 - 350 µm | 250 - 350 µm | |
Potters Industries A-Series P-0140 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 250 µm | 250 µm | mean resin; SABIC Method |
SABIC Innovative Plastics Geloy INP983 ASA SABIC INP983 is a 32% polybutyl acrylate rubber grafted weatherable ASA modifier resin. Provides excellent impact, heat distortion and weatherability properties. Maintains polymer properties in UV a.. |
|||
Particle Size | >= 250 µm | >= 250 µm | 4%; Geon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension CG E 44 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® CG E44 is a homopolymer specialty suspension resin intended for use in lowering the gloss of extruded or plastisol parts. This resin provides low surface gloss and texturing effects for flexi.. |
|||
Particle Size | >= 250 µm | >= 250 µm | 4%; Geon® DFT 1466; Internal Method |
PolyOne Geon™ Specialty Suspension Impel S100 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Impel S100 is a homopolymer specialty suspension resin intended for use in highly plasticized extrusion and injection molding formulations. It gives superior plasticizer absorption properties.. |
|||
Particle Size | 250 µm | 250 µm | 0.5% max, wet sieve |
Magyar Aluminum ALO-P90 Alumina Alumina for Polishing |
|||
Particle Size | 250 µm | 250 µm | 0.5% max, wet sieve |
Magyar Aluminum ALO-P95 Alumina Alumina for Polishing |
|||
Particle Size | 250 µm | 250 µm | |
Momentive Performance Materials AC6103 Boron Nitride (BN) Powder Agglomerate of hexagonal BN crystals. AC6103 powders are granular with good flow and blend characteristics as well as high thermal conductivity and good lubrication qualities. Information provided.. |
|||
Particle Size | 250 µm | 250 µm | Mean |
Momentive Performance Materials HCR48 Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powder grades HCR48, HCJ48, and HCM are large, high-density agglomerates, of ~10 µm crystals, with average particle sizes between 175-275 µm and tap den.. |
|||
Particle Size | 250 µm | 250 µm | <2% greater than value; ISO 1624 |
SolVin 250SB Polyvinyl Chloride General Purpose - Rigid Made by suspension polymerization.
APPLICATIONS
Injection : moldings with complex flow paths
Pressing : mixed with VC-VAc copolymers for gramophone records
Calendering : rigid films and sheets ; use.. |
|||
Particle Size | 250 µm | 250 µm | <2% greater than value; ISO 1624 |
SolVin 258RD Polyvinyl Chloride General Purpose - Rigid Made by suspension polymerization.
APPLICATIONS
Blow extrusion : opaque or crystal-clear bottles
Injection molding : rigid articles
Calendering : opaque or crystal-clear rigid sheets
Extrusion : rig.. |
|||
Particle Size | 250 µm | 250 µm | <5% greater than value; ISO 1624 |
SolVin 260RF Polyvinyl Chloride General Purpose - Rigid Made by suspension polymerization.
APPLICATIONS
Extrusion : unplasticized PVC
- tubes/pipes
- profile
- foam
- sheet, film
- blow moldings
Calendering : unplasticized PVC
- film : high temperature p.. |
|||
Particle Size | 250 µm | 250 µm | <5% greater than value; ISO 1624 |
SolVin 263RB Polyvinyl Chloride General Purpose - Rigid Made by suspension polymerization.
APPLICATIONS
Blow extrusion : opaque or crystal-clear bottles
Calendering : opaque or crystal-clear rigid sheets
Extrusion : rigid profiles and filmsInformation pr.. |
|||
Particle Size | 250 µm | 250 µm | <2% greater than value; ISO 1624 |
SolVin 264GC Polyvinyl Chloride General Purpose - Rigid or Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized, semi-rigid and rigid profiles
- plasticized and rigid pipes
- rigid "pressure" pipes
Injection molding : plasticized and se.. |
|||
Particle Size | 250 µm | 250 µm | <2% greater than value; ISO 1624 |
SolVin 264PC Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized, semi-rigid, and rigid profiles
- plasticized and rigid pipes
- blowing of plasticized and rigid films
- rigid "pressure" p.. |
|||
Particle Size | 250 µm | 250 µm | <1% greater than value; ISO 1624 |
SolVin 271DF Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized and semi-rigid profiles and pipes
- blowing of plasticized films
Calendering : opaque or transparent, plasticized and semi-r.. |
|||
Particle Size | 250 µm | 250 µm | <2% greater than value; ISO 1624 |
SolVin 271GA Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized and semi-rigid pipes for medical applications
- plasticized film for blood bags
Injection molding : plasticized and semi-rig.. |
|||
Particle Size | 250 µm | 250 µm | <2% greater than value; ISO 1624 |
SolVin 271PC Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized and semi-rigid profiles and pipes
- blowing of plasticized films
Calendering : opaque or transparent, plasticized and semi-r.. |
|||
Particle Size | 250 µm | 250 µm | <2% greater than value; ISO 1624 |
SolVin Vinidur® 464SZ Polyvinyl Chloride grafted copolymer TYPE
Suspension graft copolymer of vinylchloride and an acrylate elastomer. Vinidur 464SZ has been developed for the extrusion of window profiles with high impact strength and good weathering proper.. |
|||
Particle Size | <= 250 µm | <= 250 µm | 10% Max; 540MA3C5E |
Solvay MIRAPOL® SURF-S 410 Surfactant Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â.. |
|||
Particle Size | 250 µm | 250 µm | Before Conversion |
Silberline Sparkle Silvet® 730-30-E1 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final .. |
|||
Particle Size | 250 µm | 250 µm | 99.5 min, 60 mesh; TI-2087 |
Solvay RHODICARE T Surfactant Description: Rhodicare® T is high purity grade specifically designed for thickening and suspension in clear formulations. It has high electrolyte stability over a wide range of pH and fast hydrat.. |
|||
Particle Size | 250 µm | 250 µm | 99.5 min, 60 mesh; TI-2087 |
Solvay RHODICARE XC Surfactant Description: Rhodicare® XC is similar to standard Xanthan Gum, this grade displays improved microbial specifications. It has high electrolyte stability over a wide range of pH and fast hydration .. |
|||
Particle Size | <= 250 µm | <= 250 µm | 1; TI-2087 |
Solvay RHODOPOL® T Surfactant Description: Transparent grade xanthan gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent.Identification: XANTHAN GUMCAS: 11138 – 66 – 2Available.. |
|||
Particle Size | >= 250 µm | >= 250 µm | d50, 83%, Vibrated sieving |
TIMCAL TIMREX® KS150-600SP Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 250 µm | 250 µm | 1% above |
BorsodChem ONGROVIL S-494 Suspension PVC-Resin S-494 is a suspension type PVC homopolymer of high molecular mass. It is characterized by a porous particle structure and a narrow range of particle size. It retains its excellent pourability even a.. |
|||
Particle Size | 250 µm | 250 µm | 5% above |
BorsodChem ONGROVIL S-5167 Suspension PVC-Resin S-5167 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It r.. |
|||
Particle Size | 250 µm | 250 µm | D50 Sieve measurement; Internal Method |
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU)
(Unverified Data**) Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing.. |
|||
Particle Size | 250 µm | 250 µm | D50 Sieve measurement; Internal Method |
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU)
(Unverified Data**) Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing .. |
|||
Particle Size | 250 µm | 250 µm | 1% above |
BorsodChem ONGROVIL S-5258 Suspension PVC-Resin S-5258 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It r.. |
|||
Particle Size | 250 µm | 250 µm | <2% greater than value; ISO 1624 |
SolVin 460SL Polyvinyl Chloride grafted copolymer Made by suspension polymerization. Special product for calendered film from the high temperature process.
APPLICATIONS
Calendering : unplasticized PVC
- film : high temperature process
Extrusion : u.. |