Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sinotek Materials Soft Graphite Ring

Category Carbon , Graphite
Manufacturer Sinotek Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sinotek Materials Soft Graphite Ring.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used for electrode joint.Information provided by Sinotek
Physical Properties Metric English Comments
Density 0.0800 - 0.100 g/cc
0.00289 - 0.00361 lb/in³
Copyright © lookpolymers.com All Rights Reserved