Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlthane® 11T75D is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, with extremely high hardness. It is especially recommended for use in producing technical parts by injection molding.Applications: Pearlthane 11T75D can be used for injection molding of a variety of technical parts. It can also be applied as base resin for extremely tough (glass reinforced) engineering compounds.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D-792
Moisture Absorption at Equilibrium <= 0.10 %
<= 0.10 %
MQSA 44
Melt Flow 10 g/10 min

@Load 21.6 kg,
Temperature 198 - 208 °C
10 g/10 min

@Load 47.6 lb,
Temperature 388 - 406 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
ASTM D-2240
Tensile Strength 50.03 MPa
7256 psi
ASTM D-412
Tear Strength 230 kN/m
1310 pli
Die C; ASTM D-624
Thermal Properties Metric English Comments
Melting Point 198 - 208 °C
388 - 406 °F
Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111
Processing Properties Metric English Comments
Feed Temperature 215 °C
419 °F
Nozzle Temperature 225 °C
437 °F
Mold Temperature 35.0 °C
95.0 °F
Descriptive Properties Value Comments
Compression Zone Temperature 428°F
Metering Zone Temperature 437°F