Silon Tabond 5010 Adhesive Resin

Category Polymer , Adhesive , Thermoplastic , Polypropylene (PP)
Manufacturer Silon
Trade Name Tabond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silon Tabond 5010 Adhesive Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tabond 5010 is a a chemically modified Polypropylene. This grade is for sheets and bottles composed of Polypropylene (PP) and EVOH or PA.Characteristics: • Strong adhesion to PA / PP and EVOH / PP • Adhesion durability • Polyolefin like properties and processing • Easy handling during extrusionInformation provided by Silon
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
Melt Flow 3.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
15s
Tensile Strength, Yield 31.6 MPa
4580 psi
Elongation at Break >= 355 %
>= 355 %
Thermal Properties Metric English Comments
Melting Point 161 °C
322 °F
DSC
Descriptive Properties Value Comments
Color White