Silberline Sparkle Silver® 5271-AR

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Sparkle Silver®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Sparkle Silver® 5271-AR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sparkle Silver® 5271-AR is medium, non-leafing aluminum pigment. It is distinguished by a closely controlled particle size distribution. This results in a fine, white, face tone with silvery patina, coupled with a very deep flop effect. The clear, clean metallic colors produced are ideal for automotive paints, especially higher solids formulations.Applications: Automotive
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
Bulk Factor 0.082
0.082
Volatiles 36 %
36 %
Particle Size 19 µm
19 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
0.01% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits/High Flash