Material Notes:
General purpose compound recommended for extrusion applications. Contains a biocide and is UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.39 g/cc
1.35 - 1.39 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88
82 - 88
delayed; ASTM D-2240
Tensile Strength, Yield 16.9 MPa
2450 psi
ASTM D-638
Elongation at Yield 325 %
325 %
ASTM D-638
100% Modulus 0.00931 GPa
1.35 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F