Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 19 µm | 19 µm | |
Imerys Minsilsparâ„¢ Feldspar Minsilspar is a 170 mesh feldspathic sand (sandspar) used primarily in the Sanitaryware industry.Information provided by Imerys |
|||
Particle Size | 19 - 23 µm | 19 - 23 µm | 10% |
H.C. Starck Amperit® 586.054 Chromium Carbide-Nickel Chromium 80-20 (Cr3C2-NiCr) |
|||
Particle Size | 19 µm | 19 µm | |
Silberline 4-Allâ„¢ LEP 20051 The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr.. |
|||
Particle Size | 19 µm | 19 µm | |
Silberline SilBerCote® 5745-20Y SilBerCote® Y polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. SilBerCote® Y imparts add.. |
|||
Particle Size | 19 µm | 19 µm | |
Silberline Silvex® 113-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 19 µm | 19 µm | |
Silberline Silvex® 115-20-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 19 µm | 19 µm | |
Silberline Sparkle Silver® 5271-AR Sparkle Silver® 5271-AR is medium, non-leafing aluminum pigment. It is distinguished by a closely controlled particle size distribution. This results in a fine, white, face tone with silvery pati.. |
|||
Particle Size | 19 µm | 19 µm | |
Silberline Sparkle Silver® 5742 Sparkle Silver® 5742 is a fine, bright, regular purity, non-leafing aluminum pigment with good opacity for solvent-based general industrial coatings.Applications: Automotive |
|||
Particle Size | 19 µm | 19 µm | |
Silberline Sparkle Silver® 5745 Sparkle Silver® 5745 is a fine, regular purity, non-leafing aluminum pigment with good opacity for solvent-based general industrial coatings. It provides excellent distinctiveness of image (D.O.I.. |
|||
Particle Size | 19 µm | 19 µm | Before Conversion |
Silberline Silvet® 110-20-E Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatible with.. |
|||
Particle Size | 19 - 21 µm | 19 - 21 µm | D50 |
Sinotek Materials ZSG-20 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Particle Size | 19 µm | 19 µm | median |
Esstech V-117-1190 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |
|||
Particle Size | 19 µm | 19 µm | 10th% |
3M S38HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |