Indium Corp. #1210 Battery Flux

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. #1210 Battery Flux.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesWide process windowLow fumingMinimal residueMinimizes corrosion#1210 Battery Flux was specially formulated for high volume cast-on-strap manufacturing where rapid evaporation of solvent is necessary. This flux contains no chlorides, heavy metals or organic acids, which could affect the long term life of the batteries. #1210 Battery Flux provides excellent metallurgical fusing of all lead-based battery alloys as employed in the cast-on-strap process systems. #1210 Battery Flux exhibits very low fuming or smoke during process of manufacturing. This flux leaves very minimal residue after the burn-in process.Characteristics:Color - yellowOdor - AlcoholicInformation provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 1.045 g/cc

@Temperature 15.5 °C
1.045 g/cc

@Temperature 59.9 °F
1.104 g/cc

@Temperature 25.0 °C
1.104 g/cc

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point 29.4 °C
85.0 °F
TCC