Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinil Chemical SHINFLAME PC/ABS/GF Flame Retardant Polymer Housing

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Glass Fiber Filled , Polycarbonate (PC)
Manufacturer Shinil Chemical
Trade Name SHINFLAME
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinil Chemical SHINFLAME PC/ABS/GF Flame Retardant Polymer Housing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to produce high performance SHINFLAME compound. SHINFLAME compounds comprise halogen or non halogen flame retardant additives in engineering thermoplastics. SHINFLAME provides a wide range of the flame performance (V0, V1, V2, HB etc), mechanical and physical properties to create the application-specific environment.Feature and BenefitsExcellent fire performanceNon halogen FR availableEnvironmentally friendlyRoHS compliance (selected grade)Outstanding mechanical propertiesImproved thermal propertiesEasy processingNon toxicInformation Provided by Shinil Chemical Industry Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 97.1 MPa
14100 psi
Elongation at Break 4.0 %
4.0 %
Flexural Strength 142.2 MPa
20630 psi
Flexural Modulus 6.96 GPa
1010 ksi
Izod Impact, Notched 0.883 J/cm
1.65 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
Flammability, UL94 V-0
V-0