Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.96 GPa @Temperature 150 °C |
1010 ksi @Temperature 302 °F |
ASTM D790 |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2313 PEI 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region... |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi.. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC (Asia Pacific) LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | |
Shinil Chemical SHINFLAME PC/ABS/GF Flame Retardant Polymer Housing SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | |
Shinil Chemical SHINSTRA PC/ABS SCV2030 Structural Polymer Housing SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF006 PA 6 LNP THERMOCOMP* PF006 is a compound based on Nylon 6 resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 LNP THERMOCOMP* PF006S is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 LNP THERMOCOMP* PF006U is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of thie grade are: UV Stabilized. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 6.96 GPa | 1010 ksi | |
Phenolic 46%, Carbon fabric 54% Phenolic - Monsanto "SC 1008". Carbon fabric - "VCA" |