Material Notes:
SABIC INP388 is a high heat ASA resin, and is based on alphamethyl styrene acrylontrile butylacrylate styrene (AMS-ASA) and polybutyl arylate rubber.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Volatiles 0.20 %
0.20 %
Total NA Volatiles; SABIC Method
Particle Size 300 µm
300 µm
SABIC Method
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ASTM D2240
Descriptive Properties Value Comments
Rubber 20%
SABIC Method