Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones KSG-210 Fluid

Category Fluid , Lubricant , Silicone Base
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KSG-210 Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Mechanical Properties Metric English Comments
Penetration 400
400
Optical Properties Metric English Comments
Refractive Index 1.403
1.403
Descriptive Properties Value Comments
Crosspolymer PE crosslinked
Diluent (%) 24
DMF A 6cs
INCI Dimethicone/PEG-10/15 Crosspolymer
Copyright © lookpolymers.com All Rights Reserved