Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Verton UV00A PPA

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Verton UV00A PPA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.63 g/cc
0.0589 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 245 MPa
35500 psi
ISO 527
Elongation at Break 1.5 %
1.5 %
ISO 527
Tensile Modulus 20.36 GPa
2953 ksi
1 mm/min; ISO 527
Flexural Strength 359 MPa
52100 psi
ISO 178
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
Izod Impact, Notched (ISO) 38.0 kJ/m²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 17.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
9.89 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 22.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 276 °C
529 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following: