Material Notes:
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for low density and low thermal conductivity, and are helpful in conserving heat energy thus reducing fuel costs.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density <= 0.850 g/cc
<= 0.0307 lb/in³
Dried at 110°C
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000392 GPa
0.0569 ksi
Dried at 110°C
0.000294 GPa

@Treatment Temp. 1100 °C
0.0426 ksi

@Treatment Temp. 2010 °F
0.000294 GPa

@Treatment Temp. 3400 °C
0.0426 ksi

@Treatment Temp. 6150 °F
Compressive Strength 0.392 MPa
56.9 psi
Fired at 800°C, Cold Crushing
0.588 MPa
85.3 psi
Fired at Service temp. of 1100°C, Cold Crushing
1.18 MPa
171 psi
Dried at 110°C, Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity <= 0.163 W/m-K

@Temperature 500 °C
<= 1.13 BTU-in/hr-ft²-°F

@Temperature 932 °F
Component Elements Properties Metric English Comments
Al2O3 >= 32 %
>= 32 %
Fe2O3 <= 8.5 %
<= 8.5 %
Descriptive Properties Value Comments
Permanent Linear Change -1.0 - 1.0%
Fired at 800°C
-1.6 - 1.6%
Fired at Service temp. 1100°C