Polymer Property : Modulus of Rupture = 0.000294 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000294 GPa

@Treatment Temp. 1100 °C
0.0426 ksi

@Treatment Temp. 2010 °F
Sharadaa Ceramics REFINSUL ZAP-014 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..
Modulus of Rupture 0.000294 GPa

@Treatment Temp. 3400 °C
0.0426 ksi

@Treatment Temp. 6150 °F
Sharadaa Ceramics REFINSUL ZAP-014 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..