Shandong Guangyin GA4S11 Nylon Coating Material

Category Polymer , Thermoplastic , Nylon
Manufacturer Shandong Guangyin
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Guangyin GA4S11 Nylon Coating Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features and Applications: Wear resistance, higher strength, better tenacity, strong adhesion and better low temperature resistance. It is applicable to surface coating of wires, cables, optical cables, metal wires or ropes.Information provided by Shandong Guangyin
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
Elongation at Break 300 %
300 %
Izod Impact, Notched (ISO) NB
NB
Izod Impact, Unnotched (ISO) NB
NB
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %