Material Notes:
Low temperature service Nitrile; plasticizer freeInformation provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 75
>= 75
ASTM D2240, Type A
85
85
AVG; ASTM D2240, Type A
90

@Temperature 100 °C,
Time 252000 sec
90

@Temperature 212 °F,
Time 70.0 hour
After Dry Heat Aging; ASTM D865
Tensile Strength at Break >= 13.8 MPa
>= 2000 psi
ASTM D412 Method A
21.02 MPa
3048 psi
AVG; ASTM D412 Method A
21.06 MPa

@Temperature 100 °C,
Time 252000 sec
3054 psi

@Temperature 212 °F,
Time 70.0 hour
ASTM D865
Tensile Strength, Yield >= 4.14 MPa
>= 600 psi
Stress at Elongation M50; ASTM D412 Method A
5.41 MPa
784 psi
AVG Stress at Elongation M50; ASTM D412 Method A
>= 10.3 MPa
>= 1500 psi
Stress at Elongation M100; ASTM D412 Method A
12.51 MPa
1814 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 150 %
>= 150 %
ASTM D412 Method A
172 %
172 %
AVG; ASTM D412 Method A
189.2 %

@Temperature 100 °C,
Time 252000 sec
189.2 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D865
Compression Set 4.0 %

@Temperature 100 °C,
Time 79200 sec
4.0 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D395, Test B
9.0 %

@Temperature 100 °C,
Time 252000 sec
9.0 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395, Test B
Processing Properties Metric English Comments
Shelf Life 120 Month
120 Month
ASTM D395, Test B
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 39
Users viewing this material also viewed the following: