Polymer Property : Tensile Strength at Break = 21.02 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.02 MPa
3048 psi
AVG; ASTM D412 Method A
Seals Eastern 5488 Nitrile Rubber
Low temperature service Nitrile; plasticizer freeInformation provided by Seals Eastern, Inc.