Tensile Strength, Yield 5.41 MPa
784 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 5488 Nitrile Rubber
Low temperature service Nitrile; plasticizer freeInformation provided by Seals Eastern, Inc.