Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schmelzer Industries Curveil 220-30 Fiberglass Veil

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Schmelzer Industries
Trade Name Curveil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmelzer Industries Curveil 220-30 Fiberglass Veil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good for curved applications - drapable and flexible. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. The 200 series contains a binder additive. Data provided by the manufacturer, Schmelzer Industries.
Mechanical Properties Metric English Comments
Hardness, Barcol 36
36
Tensile Strength, Ultimate 23.11 MPa
3352 psi
s.d. 2.17 MPa, test specimen 1.23 cm wide (s.d. 0.008 cm), 0.21 cm thick (s.d. 0.008 cm)
Elongation at Break 0.56 %
0.56 %
Elongation at max. load, 0.56%
Elongation at Yield 0.53 %
0.53 %
Modulus of Elasticity 4.68 GPa
679 ksi
std. dev. 0.31 GPa
Flexural Strength 39.6 MPa
5740 psi
s.d. 3.0 MPa, specimen 2.48 cm wide (s.d. 0.02 cm), 0.21 cm thick (s.d.01 cm), 3.8 cm span (s.d. 0 cm). Test conditions: Humidity 50%, Temp. 23°C.
Flexural Modulus 3.60 GPa
522 ksi
Tangent
Users viewing this material also viewed the following: