Mechanical Properties Metric English Comments
Modulus of Elasticity 4.68 GPa
679 ksi
std. dev. 0.31 GPa
Schmelzer Industries Curveil 220-30 Fiberglass Veil
Good for curved applications - drapable and flexible. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. The 200 series contains a binder additive. ..