Material Notes:
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.211 is an impact grade.Applications:Automotive knob types, door handles and mirror housingsConnectorsCable tiesHarness clipsTubesFastenersCastor wheelsHose clipsVacuum hoseHood stayInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Water Absorption 1.3 %
1.3 %
ASTM D570
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 62.8 MPa
9100 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 142 MPa
20600 psi
ASTM D790
Flexural Modulus 7.99 GPa
1160 ksi
ASTM D790
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 217 °C
423 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648