Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in telephones, vacuum cleaners and electric fan standsInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Melt Flow 3.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Yield 39.2 MPa
5690 psi
5 mm/min; ASTM D638
Flexural Strength 59.8 MPa
8670 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 2.06 J/cm

@Thickness 6.35 mm
3.86 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C

@Thickness 6.40 mm
183 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 96.0 °C
205 °F
B/50; ISO R306