Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polycyclohexylenedimethylene Terephthalate (PCT) , Polycyclohexylenedimethylene Terephthalate (PCT), 40% Glass Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.63 g/cc
1.63 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 1.20 kg,
Temperature 300 °C
20 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Ash 40.5 %
40.5 %
ASTM D5630
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.8 MPa
8820 psi
5 mm/min; ASTM D638
Elongation at Break 1.5 %
1.5 %
5 mm/min; ASTM D638
Flexural Strength 78.5 MPa
11400 psi
2.8 mm/min; ASTM D790
Flexural Modulus 7.55 GPa
1100 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.294 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.551 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
0.294 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.551 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
1.47 J/cm

@Thickness 6.35 mm,
Temperature -30.0 °C
2.76 ft-lb/in

@Thickness 0.250 in,
Temperature -22.0 °F
ASTM D256
1.57 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
2.94 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C

@Thickness 6.40 mm
482 °F

@Thickness 0.252 in
ASTM D648
Optical Properties Metric English Comments
Yellow Index 4.0 %

@Thickness 3.20 mm
4.0 %

@Thickness 0.126 in
ASTM D1925