Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.47 J/cm @Temperature 23.0 °C |
2.76 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyMirae Moplen EP400M Injection Molding Grade Polypropylene Moplen EP400M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP400M is a block copolymer selected by customers for use in in.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature -40.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature -40.0 °F |
ASTM D256 |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature -40.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature -40.0 °F |
ASTM D256 |
LG Chemical KEYFLEX BT HB9255D Ester Type TPE Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical Lupox® TE5000HU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 26062-94-2, 137050-02-03 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical Lupox® TE5000SP PBT+PC Description: Injection Molding, PBT+PC, Low Gloss, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® BF-0370 MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® HR-0370F ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0951 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® HR-0370F ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0951 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0957 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LH-1070W PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm |
2.76 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm |
2.76 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade Very High Flow, Medium Impact GradeInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM17V ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade Very High Flow, Medium Impact GradeInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM21V ABS Injection Molding Grade Super High Gloss, High RigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm |
2.76 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm |
2.76 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LH-1070W PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR404T ABS, Heat Resistance Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
2.76 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm |
2.76 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali |