Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® CF-1070 PC, Unreinforced High Impact

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Impact Modified
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® CF-1070 PC, Unreinforced High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High-impact material for the exterior material of mobile phoneInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Melt Flow 13 g/10 min

@Load 10.0 kg,
Temperature 250 °C
13 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Flexural Strength 83.4 MPa
12100 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.96 GPa
284 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 5.39 J/cm

@Thickness 6.35 mm
10.1 ft-lb/in

@Thickness 0.250 in
ASTM D256
6.86 J/cm

@Thickness 3.17 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 138 °C
280 °F
B/50; ISO R306
Flammability, UL94 V-2

@Thickness 0.800 - 3.00 mm
V-2

@Thickness 0.0315 - 0.118 in
Copyright © lookpolymers.com All Rights Reserved