Saint-Gobain Normount® V2000 High-density Polyurethane Foam/High-performance Acrylic Adhesive Bonding Tape

Category Polymer , Adhesive , Tape , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Normount®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Normount® V2000 High-density Polyurethane Foam/High-performance Acrylic Adhesive Bonding Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Normount® V2000 series bonding tapes combine a high density, closed cell polyurethane foam substrate with a high performance acrylic adhesive on both sides. Normount® foam substrate absorbs vibrations and distributes stress forces over the entire bond line. The closed cell structure also allows the V2000 series to be used as a gasket for applications in severe environments. The high strength adhesive increases its overall capabilities. Normount® V2000 bonding tapes offer resistance against weathering, fungi, UV light, oxidation, and extreme temperatures.Features/Benefits:Higher shear strengthExcellent for die-cuttingHigh-strength, durable acrylic adhesive for long term bondSuperior aging propertiesComplete compatibility with polycarbonates, acrylic plastics and most silicones testedTypical Industrial Bonding Applications: Vibration dampeners, weatherstripping, appliance handles, circuit board mounts, mirror mounting (additional support recommended), glass lamination, letters and signs, emblems and nameplates. Typical Construction Bonding Applications: Skylights, trim and ornamentation, sound baffles, HVAC gasketing, kick panels, signs, glass lamination (requiring closed cell). All data based on a 0.03 inch test sample.(Available in multiple thicknesses.) Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 0.498 g/cc
0.0180 lb/in³
ASTM D1667
Water Absorption 5.0 %
5.0 %
% by weight; NTP-36
Mechanical Properties Metric English Comments
Hardness, Shore A 20
20
ASTM D2240
Tensile Strength, Yield 1.76 MPa
255 psi
ASTM D-412 (Die C)
Elongation at Break 240 %
240 %
ASTM D-412 (Die C)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Descriptive Properties Value Comments
Color Black