Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.76 MPa | 255 psi | ASTM D-412 (Die C) |
Saint-Gobain Normount® V2000 High-density Polyurethane Foam/High-performance Acrylic Adhesive Bonding Tape Description: Normount® V2000 series bonding tapes combine a high density, closed cell polyurethane foam substrate with a high performance acrylic adhesive on both sides. Normount® foam substra.. |