Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -30.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Continuous
Dielectric Polymers TRANS-SIL® NT-1001 Silicone Transfer Adhesive  (discontinued **)
Crosslinked silicone adhesive with 2 polyester film release liners.Features: Resistant to extreme temperaturesHigh bond strengthChemical resistantApplications: High performance bonding and other app..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Garlock 361 Nitrile Sheet Rubber
Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #361 has a higher tensile strength and is a superior product in applications requiring ..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Garlock 363 Nitrile Sheet Rubber
Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #363 is a good quality, oil-resistant nitrile sheet.Information provided by Garlock Rub..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Garlock 509 Butyl Sheet Rubber
Style #509 is a branded, chloro-butyl sheet rubber product.Information provided by Garlock Rubber Technologies
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Garlock 7797 Neoprene Sheet Rubber
This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth cloth finishInformation provided by Garlock Rubber Technologies
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Garlock 7986 Neoprene Sheet Rubber
This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth cloth finishInformation provided by Garlock Rubber Technologies
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Approx. Cold test
Lubriplate 3000-W Moly-Lithium Type Multi-Purpose Grease
Tacky, moly-lithium, extreme pressure greases that provide a durable, tenacious, adhesive film to protect against water, rust, and corrosive contaminants. 3000-W is for cold ambient temperatures.App..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Approx. Cold test
Lubriplate 105 Calcium Type Multi-Purpose Grease
These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Appli..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Saint-Gobain Norcrylâ„¢ A1000 Solid Acrylic Bonding Tape
Description: The Norcrylâ„¢ solid acrylic core has outstanding internal strength. Norcrylâ„¢ structural grade bonding power can reduce or replace conventional fasteners, rivets, liquid adhesiv..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Saint-Gobain Norcrylâ„¢ A2000 Solid Acrylic Bonding Tape
Description: The Norcrylâ„¢ solid acrylic core has outstanding internal strength. Norcrylâ„¢ structural grade bonding power can reduce or replace conventional fasteners, rivets, liquid adhesiv..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Saint-Gobain Norton® V980 Paper Liner Pressure Sensitive Adhesive Foam Sealant
Description: Closed cell PVC foam with a pressure-sensitive adhesive on both sides. Proven Performance: Norseal® V980/V990 foam sealant combines a closed cell polyvinyl chloride foam substrate wt..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Saint-Gobain Norton® V990 Poly Liner Pressure Sensitive Adhesive Foam Sealant
Description: Closed cell PVC foam with a pressure-sensitive adhesive on both sides. Proven Performance: Norseal® V980/V990 foam sealant combines a closed cell polyvinyl chloride foam substrate wt..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Saint-Gobain Normount® V1300 White Polyurethane Foam Bonding Tape for Interior Use
Description: Normount® V1300 series bonding tapes combine a polyurethane foam substrate with a durable, pressure-sensitive acrylic adhesive on both sides. The foam properties dissipate vibrations..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Saint-Gobain Normount® V2000 High-density Polyurethane Foam/High-performance Acrylic Adhesive Bonding Tape
Description: Normount® V2000 series bonding tapes combine a high density, closed cell polyurethane foam substrate with a high performance acrylic adhesive on both sides. Normount® foam substra..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Saint-Gobain Norton® Log Home Foam® V790
Description: Provides Positive Seal in Log Home Joints: Norseal® Log Home Foam® V790 is a medium-density foam specifically developed for log home gasketing. Under a minimum of 25 percent compr..
Minimum Service Temperature, Air -34.4 °C
-30.0 °F
Continuous
Dielectric Polymers TRANS-SIL® NT-1005 Silicone Transfer Adhesive  (discontinued **)
Crosslinked silicone adhesive with 2 polyester film release liners.Features: Resistant to extreme temperaturesHigh bond strengthChemical resistantApplications: High performance bonding and other app..