STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-95-1000 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarXTRUDE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-95-1000 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: StarXTRUDE XTR-95-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & PC/ABSProcessing Method: ExtrusionInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Viscosity 17500 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
17500 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 93

@Time 10.0 sec
93

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 12.57 MPa

@Time 7200 sec
1823 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 700 %

@Time 7200 sec
700 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.007281 GPa

@Time 7200 sec
1.056 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 68.4 kN/m
390 pli
ASTM D624