Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Vanes for high loaded compressorsInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
Open Porosity 10 %
10 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
Size/Load - 5/100
Modulus of Elasticity 13.8 GPa
2000 ksi
Flexural Strength 58.6 MPa
8500 psi
Compressive Strength 148 MPa
21500 psi
Thermal Properties Metric English Comments
CTE, linear 3.96 µm/m-°C

@Temperature 20.0 °C
2.20 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 79.5 W/m-K
552 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 593 °C
1100 °F
In oxygen
Maximum Service Temperature, Inert 1204 °C
2199 °F
Reducing Atm.
Descriptive Properties Value Comments
Impregnation Salt