Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 13.8 - 36.2 GPa | 2000 - 5250 ksi | Average value: 27.5 GPa Grade Count:15 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Modulus of Elasticity | 13.8 GPa | 2000 ksi | |
Indium Corp. Indalloy® 151 Pb-Sn-Ag Solder Alloy Similar to Indalloy #165 (Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly.)Information provided by the manufacturer, Indium Corporation. |
|||
Modulus of Elasticity | 13.8 GPa | 2000 ksi | Effective Modulus |
Hardwire 12x-4-12 Low Density Composite The 12X Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 12X wire cord is used where the traits of high tensile strain, excellent conformabi.. |
|||
Modulus of Elasticity | 13.8 GPa | 2000 ksi | in <110> direction |
Mateck Potassium Bromide (KBr) Optical crystals |
|||
Modulus of Elasticity | 13.8 GPa | 2000 ksi | |
SGL Carbon Group EK 200 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 13.8 GPa | 2000 ksi | |
SGL Carbon Group EK 201 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 13.8 GPa | 2000 ksi | |
SGL Carbon Group V 1626 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Modulus of Elasticity | 13.8 GPa | 2000 ksi | |
SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |