Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 148 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 148 MPa
21500 psi
10% Def.; ASTM D695
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet)
Compressive Strength 148 MPa
21500 psi
Poco Graphite EDM-4 EDM Graphite
POCO's EDM-4 is our premier offering in the Ultrafine classification. This highly isotropic grade combines strength with moderate hardness, yielding superior electrode fabrication characteristics. T..
Compressive Strength 148 MPa
21500 psi
SGL Carbon Group EK 10 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Compressive Strength 148 MPa
21500 psi
SGL Carbon Group EK 17 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Compressive Strength 148 MPa
21500 psi
SGL Carbon Group EK 2239 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Compressive Strength 148 MPa
21500 psi
SGL Carbon Group V 1626 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Compressive Strength 148 MPa
21500 psi
ASTM D695
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
Compressive Strength 148 MPa
21500 psi
ASTM D695
Plenco 1500 Polyester, Granular, Transfer Molded
PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon..
Compressive Strength 148 MPa
21500 psi
Cosmic Plastics ID-40 Orlon Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Compressive Strength 148 MPa
21500 psi
Ultimate; TM R050-38
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett..
Compressive Strength 148 MPa
21500 psi
Break; TM R050-38
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett..
Compressive Strength 148 MPa
21500 psi
Ultimate; TM R050-38
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett..
Compressive Strength 148 MPa
21500 psi
Break; TM R050-38
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett..
Compressive Strength 148 MPa
21500 psi
ASTM D695
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
Copyright © lookpolymers.com All Rights Reserved