Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufTech™ 12-041 PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF S&E Specialty Polymers TufTech™ 12-041 PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: A PVC based semi-rigid compound designed for general purpose use in extruded form, including piping applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 68.0
<br>@Time 15.0 sec
68.0
<br>@Time 0.00417 hour
ASTM D2240
Tensile Strength, Yield 28.3 MPa
4100 psi
Type I, 0.2 in/min; ASTM D638
Flexural Modulus 0.0414 GPa
6.00 ksi
Procedure B, 0.05 in/min; ASTM D790
1.45 GPa
210 ksi
0.05 in/min; ASTM D790
Izod Impact, Notched NB
NB
Method A, 2.75 J; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 44.8 °C
113 °F
ASTM D648