Material Notes:
Formula: C4H11NCAS: 598-56-1Description: Dimethylethylamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water. Synonyms: DMEA, Dimethylethylamin, N,N-Dimethylethanamine, Ethyldimethylamin, N-Ethyl-N-methylmethanaminApplications: Intermediate used in the production of Catalyst & curative for foundry resin cores, Polyurethane catalyst, Acid binder, Stabilizer for chlorinated hydrocarbonsInformation provided by BASF
Physical Properties Metric English Comments
Density 0.676 g/cc
0.0244 lb/in³
Molecular Weight 73.1 g/mol
73.1 g/mol
Thermal Properties Metric English Comments
Melting Point -140 °C
-220 °F
Boiling Point 36.5 °C
97.7 °F
Flash Point -45.5 °C
-49.9 °F
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
DIN 51 777
Descriptive Properties Value Comments
Assay >99.5%
Color <20
APHA, DIN EN 1557
Ignition Temperature 190°C